For STS, RMG and RTG Cranes
They are replaced because of flange wear, flange breakage, and mechanical overloads characterized by pitting and spalling. Each of these in-service factors must be carefully considered before the combination of wheel design, material selection, hardness pattern and heat treating technology is selected.
Specifications
Wheel range of size available | Φ300 – 1000 mm |
Material | 42CrMo,35CrMo or according to customer requirement |
Heat treatment | Hardening and tempering, high frequency quenching, carburizing quenching and so on |
Trand surface and rim quench depth | 15 – 18 mm |
Test Reports | Present |